Shape Memory Wire

Standard:ASTM F2063,DIA:≥0.05mm

Main uses: fishing line,super elastic memory alloy mobile phone antennas,optical glasses frames, Bluetooth headsets, medical.

Shape Memory Wirenitinol wire in orthodonticsnitinol orthodontic wire

Grade:

TiNi-01 phase transition temperature: 20 ℃ -40 ℃

TiNi-02 phase transition temperature: 45 ℃ -90 ℃

TiNi-SS phase transition temperature: 5 ℃ -15 ℃

TiNi-03 phase transition temperature: <5 ℃

TiNi-YY phase transition temperature: 33 ℃ ± 3 ℃

TiNiCU phase transition temperature: As-Ms≤5 ℃

TiNiNb phase transition temperature: As-Ms <150 ℃

Physical properties of Nitinol memory wire: tensile strength: 850 MPa yield strength: 195 ~ 690 MPa

Elongation:

25 ~ 50%

Chemical composition of Nitinol memory wire:

Ni: 55.4% –56.2% C≤0.07 H≤0.005 O≤0.050 N: ≤0.05

Executive standard:

ASTM—2063—01 ASTM F2063-2000 shape memory alloy processing material